What is GH3536 superalloy (Hastelloy X alloy)

GH3536 (Hastelloy X alloy) is a nickel-based superalloy with high iron
content mainly solid solution strengthened by chromium and molybdenum. It has
good oxidation resistance and corrosion resistance, and has moderate durability
and creep below 900 ℃. Strength, cold and hot workability and good weldability.
Used in the manufacture of combustion chamber parts and other high-temperature
parts of aero-engines, long-term use below 900 °C, and short-term operating
temperature can reach 1080 °C. The main varieties supplied are plates, strips,
pipes, bars, forgings, rings and precision castings.

GH3536 (Hastelloy X alloy) process performance and requirements

GH3536 (Hastelloy X alloy) formability alloy has good cold and hot forming
properties. Forging heating temperature 1170℃±10℃, final forging temperature not
lower than 950℃; slab hot rolling heating temperature 1150℃±10℃, final rolling
temperature not lower than 850℃; ring hot rolling heating temperature 1170℃±10℃
.

GH3536 (Hastelloy X alloy) welding performance This alloy has good welding
process performance, and can be welded by argon arc welding, seam welding and
spot welding. HGH3536 or HGH3113 wire is recommended for argon arc welding.

The microstructure of the alloy in the solid solution state is an austenite
matrix with a small amount of TiN and M6C carbides. After long-term aging at
700~900℃, the main precipitation phases are M12C and M3B2, accompanied by trace
μ phase and L phase. After aging at 700℃ for 200h, a small amount of σ phase
appeared, but after aging at 800℃, the σ phase did not exist, and a small amount
of M23C6 was precipitated, and sometimes a small amount of L phase appeared.
Therefore, the alloy exhibits a certain degree of age hardening after long-term
aging, which reduces the plasticity and the high temperature strength.

About 3dprintingpassion

3dprintingpassion is a trusted global chemical material supplier & manufacturer with
over 12 years experience in providing super high-quality chemicals and
Nanomaterials. The company export to many countries, such as USA, Canada,
Europe, UAE, South Africa, Tanzania,Kenya,Egypt,Nigeria,Cameroon,Uganda,Turkey,Mexico,Azerbaijan,Belgium,Cyprus,Czech
Republic,Brazil, Chile, Argentina, Dubai, Japan, Korea, Vietnam, Thailand,
Malaysia, Indonesia, Australia,Germany, France, Italy, Portugal etc. As a
leading nanotechnology development manufacturer, 3dprintingpassion dominates the market.
Our professional work team provides perfect solutions to help improve the
efficiency of various industries, create value, and easily cope with various
challenges. If you are looking for Hastelloy X alloy powder, please send an email to:
sales2@nanotrun.com


0d2d37b7f1662f42a1c61188be58692e

(What is GH3536 Superalloy (Hastelloy X alloy))

Contact Form

Newsletter Updates

Enter your email address below and subscribe to our newsletter